NICKEL-CHROMIUM-MOLYBDENUM ALLOY

Hastelloy C-22

Hastelloy C-22 is a nickel-chromium-molybdenum-tungsten alloy designed for broad corrosion resistance in oxidizing and reducing environments. It is especially resistant to pitting, crevice corrosion and stress-corrosion cracking.

UNS N06022 SPEC ASTM B575
MATERIAL OVERVIEW

Hastelloy C-22 Information

Hastelloy C-22 is a nickel-chromium-molybdenum-tungsten alloy designed for broad corrosion resistance in oxidizing and reducing environments. It is especially resistant to pitting, crevice corrosion and stress-corrosion cracking.

Metallic winding and compatible ring components where service conditions are suitable.

UNS Number N06022
Common Product Specification ASTM B575
Material Type Ni-Cr-Mo-W corrosion-resistant alloy
Common / Applicable Specification ASTM B575 (plate/sheet/strip)
Typical Gasket Use Metallic winding and compatible ring components where service conditions are suitable.
CHEMICAL PROPERTIES

Hastelloy C-22 Chemical Composition

Reference composition limits are shown below. Exact requirements should be confirmed against the applicable product specification and certified material documentation.

Element / Constituent Symbol Composition / Information
Carbon C 0.015 max.
Chromium Cr 20.0–22.5
Molybdenum Mo 12.5–14.5
Tungsten W 2.5–3.5
Iron Fe 2.0–6.0
Cobalt Co 2.5 max.
Manganese Mn 0.50 max.
Silicon Si 0.08 max.
Vanadium V 0.35 max.
Nickel Ni Balance
MECHANICAL PROPERTIES

Hastelloy C-22 Mechanical Properties

Reference room-temperature properties are shown for a commonly supplied condition. Exact requirements depend on product form, size, heat treatment and governing specification.

Property Reference Value Unit / Basis
Tensile Strength 690 min. MPa
0.2% Offset Yield Strength 310 min. MPa
Elongation 45 min. %

Values shown are engineering reference data, not universal design allowables. Final procurement and design must use the governing specification, exact product form/condition and certified material test documentation.

ENGINEERING INFORMATION

Hastelloy C-22 Physical & Service Information

Reference physical properties and service considerations relevant to material selection for Spiral Wound Gaskets.

Density Approx. 8.7 g/cm³
Structure Nickel-base solid-solution alloy
Corrosion Behaviour Excellent resistance across a wide range of oxidizing and reducing chemical environments.
Heat Treatment Normally solution annealed.
Service Selection Verify compatibility for the exact acid, concentration, contaminants and temperature.